10 types of defects, what went wrong, and what you and your supplier can do to fix it together.


Chapters:



  1. Gas hole porosity

  2. Hydrogen gas porosity

  3. Inclusions

  4. Part design related defects

  5. Mold design related defects

  6. Mold maintenance related defects

  7. Supplier related defects


Defects include: porosity, hydrogen gas porosity, inclusions, shrink, bent, misrun, crack, rough surface finish, flash, and parting line shift.